Home/Craft
Craft · CRAFT

Craft

From raw material to laser marking — the seven steps behind every hand-blown crystal glass.

Seven Steps, One Glass

Raw Material Selection

Raw Material Selection

RAW MATERIAL

High-clarity crystal is selected and batched under controlled temperature for clarity and strength.

Melting at 1300°C

Melting at 1300°C

MELTING

Melted at 1300°C and refined until the crystal reaches the exact viscosity for blowing.

Free Blowing

Free Blowing

BLOWING

A gather on the blowpipe, one breath, a seamless body formed in a single piece.

Hand Shaping

Hand Shaping

SHAPING

The rim and the 5mm stem are shaped by hand in the flame.

Fire Polishing

Fire Polishing

POLISHING

Annealed and polished so the rim is smooth against the lips.

Rigorous Inspection

Rigorous Inspection

INSPECTION

Every glass is checked for clarity and wall consistency; anything uneven is discarded.

Laser Marking

Laser Marking

LASER MARK

Only those that pass every step receive the RE mark.